SPECIFICATION:Standard & MaterialCarbon SteelASTM A519 StandardMT1010, MT1020, 1008, 1010, 1018, 1020, 1025, 1030, 1045, 1518JIS G3445 StandardSTKM11A STKM12A STKM12B STKM12C STKM13A STKM13B STKM13C STKM14A STKM14B STKM14C STKM15A STKM15C STKM16A STKM16C STKM17A STKM17C STK......
Standard & Material | Carbon Steel | ASTM A519 Standard | MT1010, MT1020, 1008, 1010, 1018, 1020, 1025, 1030, 1045, 1518 |
JIS G3445 Standard | STKM11A STKM12A STKM12B STKM12C STKM13A STKM13B STKM13C STKM14A STKM14B STKM14C STKM15A STKM15C STKM16A STKM16C STKM17A STKM17C STKM18A STKM18B STKM18C STKM19A STKM19C STKM20A | ||
JIS G3473 Standard | STC370, STC440, STC510A, STC510, STC540, STC590A, STC590B | ||
DIN 2391 Standard | St 35, St45, St52 | ||
EN 10297-1 Standard | E235, E275, E315, E355, E470 | ||
EN 10305-1 Standard | E215, E235, E355 | ||
EN 10305-4 Standard | E215, E235, E355 | ||
BS 6323-3 Standard | HFS 3, HFS 4, HFS 5, HFS 8 | ||
NF A49-311 | TU 37-b, TU 52-b, TU 56-b, TU XC35 | ||
Alloy Steel | ASTM A519 Standard | 1345, 3140, 4130, 4135, 4140, 4150, 4320, 4340, 5120, 5130 | |
JIS G3429 Standard | STH11, 12 STH21, 122 STH31 | ||
JIS G3441 Standard | SCR420TK, SCM415TK, SCM418TK, SCM420TK, SCM430TK, SCM440TK | ||
Stainless Steel | ASTM A511 Standard | MT304, MT304L, MT310S, MT316, MT316L, MT317, MT321, MT347, MT403, MT410, MT431 | |
ISO Standard | NACE MR-0175 | ||
Size | Size Range | Tolerance | |
OD | 6-325mm | -0.035 -- +0.045mm | |
ID | 2-250mm | ±0.035mm | |
WT | 1-32mm | depends on sizes | |
Length | random or fixed length | +0-3.5mm | |
Straightness | 0.15:1000, 0.4:1000, 0.5:1000 1:1000 or customized | ||
Surface Roughness | Ra 0.02-0.4μm |
Steel Grade | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Nb/V(%) |
STKM11A | ≤0.12 | ≤0.35 | ≤0.60 | ≤0.040 | ≤0.040 | - |
STKM12A | ≤0.20 | ≤0.35 | ≤0.60 | ≤0.040 | ≤0.040 | - |
STKM12B | ≤0.20 | ≤0.35 | ≤0.60 | ≤0.040 | ≤0.040 | - |
STKM12C | ≤0.20 | ≤0.35 | ≤0.60 | ≤0.040 | ≤0.040 | - |
STKM13A | ≤0.25 | ≤0.35 | 0.30~0.90 | ≤0.040 | ≤0.040 | - |
STKM13B | ≤0.25 | ≤0.35 | 0.30~0.90 | ≤0.040 | ≤0.040 | - |
STKM13C | ≤0.25 | ≤0.35 | 0.30~0.90 | ≤0.040 | ≤0.040 | - |
STKM14A | ≤0.30 | ≤0.35 | 0.30~1.00 | ≤0.040 | ≤0.040 | - |
STKM14B | ≤0.30 | ≤0.35 | 0.30~1.00 | ≤0.040 | ≤0.040 | - |
STKM14C | ≤0.30 | ≤0.35 | 0.30~1.00 | ≤0.040 | ≤0.040 | - |
STKM15A | 0.25~0.35 | ≤0.35 | 0.30~1.00 | ≤0.040 | ≤0.040 | - |
STKM15C | 0.25~0.35 | ≤0.35 | 0.30~1.00 | ≤0.040 | ≤0.040 | - |
Steel Grade | Tensile Strength(N/mm²) | Yield Strength(N/mm²) |
STKM11A | ≥290 | - |
STKM12A | ≥340 | ≥175 |
STKM12B | ≥390 | ≥275 |
STKM12C | ≥470 | ≥355 |
STKM13A | ≥370 | ≥215 |
STKM13B | ≥440 | ≥305 |
STKM13C | ≥510 | ≥380 |
STKM14A | ≥410 | ≥245 |
STKM14B | ≥500 | ≥355 |
STKM14C | ≥550 | ≥410 |
STKM15A | ≥470 | ≥275 |
STKM15C | ≥580 | ≥430 |
+C(BK) | Cold drawn/hard.After the last cold forming,no heat treatment. |
+LC(BKW) | Cold drawn/soft.After the last heat treatment follows the cold drawing there is a light finishing pass. |
+SR(BKS) | Cold drawn and stress relieved annealed. After the final cold drawing process the tubes are stress relieved annealed in a controlled atmosphere. |
+A(GBK) | After the final cold drawing process the tubes are stress relieved annealed in a controlled atmosphere. |
+N(NBK) | Normalized. After the last cold drawing process the tubes are annealed in a controlled atmosphere. |